Steel bluing
All work should be carried out in a well-ventilated room, using protective gloves
1) If necessary, remove previous blackening and corrosion with the Bluing and Rust Remover: shake the bottle, apply the remover, leave for 10-20 minutes and then wipe dry with a cloth.

2) Degrease the surface with Cleaner

3) Shake the GunBlasky product and apply it to the surface with a cloth, swab or cotton swab. After a few seconds, rinse off excess product with water and wipe the surface dry.

4) Treat the surface again, rinse and wipe. It is usually enough to apply 2-3 coats to achieve a beautiful matte black surface.

5) Be sure to apply ProtectiveOil or neutral GunOil.

Aluminum bluing
All work should be carried out in a well-ventilated room, using protective gloves
1) Degrease the surface with Cleaner

2) Then apply AluminumBlack with a cotton swab or cloth using light pressure and rubbing.

3) Rinse off the excess with water and wipe the surface with a dry cloth with a little pressure.

4) Also apply a second coat and so on. Usually 4 layers are enough. Once the blackening is complete, the coating should not be rubbed off with a dry cloth.

5) Apply ProtectiveOil or neutral GunOil.

Copper, brass and bronze bluing
All work should be carried out in a well-ventilated room, using protective gloves
1) Degrease the surface with Cleaner.

2) Then apply a thin layer of BrassBlack using a cotton swab or cloth.

3) Rinse off excess product with water and wipe dry.

4) If necessary, also apply a second coat.